  • Tantalum bolts for hot phosphoric acid

    Q: I’m running a semiconductor wet chemical etching process that utilizes 85 % phosphoric acid at around 150-160°C. I need a material that can withstand this process. Super Duplex hex bolts are not cutting it. A: At that particular concentration and temperature high performance nickel alloys like Hastelloy C276 bolts…

    Continue reading
  • Hastelloy C22 fasteners used in wet chloride

    Q: I have a waste water purifying situation where I’m using chlorine to treat the water. In addition to the acidic solution produced the fastener will also experience high loads, so I’m also concerned with stress corrosion cracking. Currently Super Duplex 2507 is not doing the job. Any recommendations on…

    Continue reading
  • Duplex 2205 and Hastelloy fasteners in pulp & paper digester

    Q: We have a pulp & paper digester that is used to cook wood chips in an alkaline solution. The fasteners will be exposed to high temperatures and abrasive conditions. Any suggestions? A: Without knowing the specifics of your process, I can make two general material suggestions. Duplex 2205 fasteners…

    Continue reading
  • Titanium grade 5 bolts for lightweight robotic application

    Q: I have a robotic application where I need a fastener that is both lightweight and strong. Also, the style of the fastener needs to provide a wide clamping area in a low clearance area. Any suggestions? A: A material you might consider is Titanium, grade 5. The most common…

    Continue reading
  • Hastelloy B2 vs B3 bolts: Whats the difference?

    Q: Is there any advantage of using a Hastelloy B3 fastener over a B2 fastener? A: Both Hastelloy B2and B3 fasteners provide good resistance to non-oxidizing acids, such as hydrochloric acid and sulfuric acid. The only advantages of Hastelloy B3 fasteners over B2, is that they offer enhanced thermal stability…

    Continue reading
  • Molybdenum screws temperature limit explained

    Q: I saw on your high temperature chart that Molybdenum is listed twice. I’m confused, which high temperature should I use? A: Both high temperatures are accurate, depending on the situation where you are using Molybdenum fasteners. Molybdenum screws can be used up to 2912F only if it is used…

    Continue reading
  • Difference between Incoloy 825 and 925 bolts

    Q: What is the difference between Incoloy 825 and 925 bolts? A: Bolts made from Incoloy 925 are precipitation hardened version of Incoloy 825 bolts. What this means is it is put through a heat treatment process which hardens the alloy at the atomic level. Basically Incoloy 925 bolts offers…

    Continue reading
  • Difference between Monel 400 and Monel K500 bolts

    Q: I’m currently using Monel 400 hex head bolts in salt water. Should I be using K500? What’s the difference? A: Basically, Monel K500 is a precipitation hardened version of Monel 400. This means the material goes through a heat treating process that changes the alloy’s structural matrix to increase…

    Continue reading
  • Best creep resistance polymer fastener

    Q: How does creep occur and what polymer is best to prevent this? A: Creep is the permanent deformation of the material caused by constant load or stress, usually accompanied by constant high temperature. This can result in permanent changes of the fastener shape as well weakening and fracturing of…

    Continue reading
  • Titanium vs Monel: Bolts for stagnant sea water

    Q: I have a seawater application where the water can be stagnant or polluted. Is Monel bolts the best choice? A: For stagnant seawater application we would usually suggest Titanium over Monel fasteners. Although Monel is very resistant to saltwater, it can experience pitting corrosion in stagnant water situations. There…

    Continue reading
  • Usable temperature limit of Inconel 718 bolts

    Q: What is the highest temperature I could use Inconel 718 bolts? A: Inconel 718 fasteners could be used reliably up to about 1300F. Because Inconel 718 is heat treated or age hardened at 1325F, going beyond 1300F will significantly affect its strength properties. Furthermore, its strength may not fully…

    Continue reading
  • Best flange for high pressure hydrochloric acid

    Q: I have a high pressure application with HCl at fluctuating temperatures. Can you recommend the best flange to provide a safe secure joint? A: Hands down, the weld neck flange is best for these types of hazardous, high pressure applications. Weld neck flanges are easily identified by their long…

    Continue reading
  • Best uses for a threaded flange

    Q: When do you recommend to use a threaded flange? I need a flange that can be changed easily & frequently. A: After speaking with the customer, I found out that he has a pilot plant where he will be frequently changing parts. In this case a threaded flange is…

    Continue reading
  • Calculating bolt break force or yield

    Q: How do I calculate the actual break force or yield of a bolt for a particular size? A: The Ultimate Tensile properties for a material like Hastelloy C276 is independent of the size of the bolt, as its based on the x-sectional area of the bolt which typically is…

    Continue reading
  • When to use a lap joint flange

    Q: When is it best to use a lap joint flange? A: Lap joint flanges are good for very expensive materials like tantalumand zirconiumand other specialty alloys like Hastelloyor Inconeldue to reduced cost of sleeve vs solid flange. Lap joint flanges are unique in that they are made of two…