Extreme Bolt & Fastener offers the highest performing engineered polymer fasteners available to industry. We have provided numerous guides to help you compare the polymers (PEEK, PFA, PTFE, PVDF, Torlon & Vespel) and their unique properties. Feel free to contact our materials experts for additional guidance and support in choosing the best material for your challenging application.
| Engineered Polymers | Resources & Guides |
|---|---|
Material Properties Chart
| Property | ASTM / UL Test | PEEK Unfilled | PEEK Glass Fiber | PEEK Carbon Fiber | Torlon® PAI 4203 | Kynar® PVDF | Vespel® Polyimide | Teflon® PTFE | Teflon® PFA |
|---|---|---|---|---|---|---|---|---|---|
| PHYSICAL | |||||||||
| Density (lb/in³) (g/cm³) | D792 | 0.047 (1.31) | 0.054 (1.49) | 0.052 (1.44) | 0.051 (1.41) | 0.064 (1.77) | 0.051 (1.43) | 0.078 (2.2) | 0.077 (2.14) |
| Water Absorption, 24 hrs (%) | D570 | 0.1 | 0.1 | 0.4 | 0.33 | 0.03 | 0.24 | < 0.01 | <0.03 |
| MECHANICAL | |||||||||
| Tensile Strength (psi) | D638 | 14,500 | 16,000 | 19,000 | 22,000 | 7,000 | 12,500 | 3,900 | 3,600 |
| Tensile Elongation at Break (%) | D638 | 20 | 2.2 | 1.2 | 7.6 | 50 | 7.5 | 300 | 330 |
| Hardness, Rockwell, R/M Scale | D785 | R126 | R126 | R126 | M120 | R80 | M90 | R58 | R55 |
| IZOD Impact Notched (ft-lb/in) | D256 | 1.6 | 1.8 | 5 | 2.7 | 3 | 0.8 | 3.5 | No Break |
| THERMAL | |||||||||
| Coefficient of Linear Thermal Expansion (x 10-5 in./in./°F) | D696 | 2.6 | 1.2 | 2 | 3.1 | 6.6 | 3 | 7.5 | 7.8 |
| Heat Deflection Temp (°F / °C) at 264 psi | D648 | 320 / 160 | 600 / 315 | 660/350 | 532 / 278 | 230 / 110 | 680 / 360 | 132 / 55 | 163 / 73 |
| Melting Temp (°F / °C) | D3418 | 644 / 340 | 644 / 340 | 649/342 | none (degrades ~500 °C | 332 / 166 | none (degrades ~500 °C) | 635 / 335 | 575 / 302 |
| Max Operating Temp (°F / °C) | - | 480 / 249 | 480 / 249 | 480 / 249 | 525/ 275 | 300/ 150 | 572 / 300 | 500 / 260 | 500 / 260 |
| Thermal Conductivity (BTU-in/ft²-hr-°F) | C177 | 1.8 | 3.0 | 1.8 | 1.2 | 2.0 | 1.7 | 1.4 | |
| ELECTRICAL | |||||||||
| Dielectric Strength (V/mil) short time, 1/8" thick | D149 | 480 | 190 | - | 580 | 1700 | 560 | 600 | 6500 |
| Dielectric Constant at 1 MHz | D150 | 3.3 | 3.7 | - | 3.9 | 8.5 | 3.55 | 2.1 | 2.03 |
| Dissipation Factor at 1 MHz | D150 | 0.003 | - | - | 0.026 | 0.015 | 0.0034 | < 0.0002 | 0.0001 |
| Volume Resistivity (ohm-cm) at 50% RH | D257 | 1016 | 1016 | 105 | > 1016 | 2x1014 | >1014 | > 1018 | > 1018 |
| APPROVALS | |||||||||
| Approval | FDA | YES | NO | NO | NO | YES | NO | YES | YES |
| Approval | USDA | YES | NO | NO | NO | YES | NO | NO | NO |
| Approval | NSF | NO | NO | NO | NO | YES | NO | NO | NO |
| Approval | 3A DAIRY | YES | NO | NO | NO | YES | NO | NO | NO |
| Approval | USP CLASS VI | Medical Grades Available | Medical Grades Available | Medical Grades Available | NO | YES | NO | Medical Grades Available | Medical Grades Available |
| Materials | Usabel Temp Limit (°F) | Usable Temp Limit (°C) |
|---|---|---|
| Engineered Polymers | ||
| PI (Vespel®) | 572 | 300 |
| PAI (Torlon®) | 527 | 275 |
| PEEK (Victrex®) | 500 | 260 |
| PTFE | 500 | 260 |
| PVDF (Kynar®) | 248 | 120 |
| Nylon (Reference) | 212 | 100 |
| Material | Ultimate Tensile (ksi) |
|---|---|
| PFA | 3.6 |
| PTFE | 3.9 |
| PVDF | 6.5-8.0 |
| Vespel | 12.5 |
| PEEK Unfilled | 14.5 |
| PEEK Glass Fiber | 16.0 |
| PEEK Carbon Fiber | 19.0 |
| Torlon Unfilled | 22.0 |
| ASTM or UL test | Victrex® PEEK | Kynar® PVDF | Teflon® PTFE / PFA | Torlon® PAI 4203 | Vespel® Polyimide |
|---|---|---|---|---|---|
| Acids | |||||
| 10% Hydrochloric Acid | A | A | A | A | A |
| 37% Hydrochloric Acid | B | A | A | A | C |
| 10% Sulfuric Acid | A | A | A | A | A |
| 50% Sulfuric Acid | C | A | A | A | C |
| 10% Nitric Acid | A | A | A | A | B |
| 50% Nitric Acid | C | B | A | - | C |
| 10% Hydrofluoric Acid | D | A | A | A | B |
| 50% Hydrofluoric Acid | C | A | A | D | C |
| 10%Phosphoric Acid | A | A | A | A | A |
| 10% Acetic Acid | A | A | A | A | A |
| 10% Citric Acid | A | A | A | A | A |
| Bases | |||||
| Ammonia gas | A | A | A | C | C |
| 10% Sodium Hydroxide | A | A | A | D | C |
| 80% Sodium Hydroxide | A | A | A | D | D |
| 10% Potassium Hydroxide | A | A | A | - | C |
| Calcium Hydroxide | A | A | A | - | D |
| Organics | |||||
| Methyl Alcohol | A | A | A | - | B |
| Isopropyyl Alcohol | A | A | A | A | A |
| Toluene | A | B | A | A | A |
| Xylene | A | A | A | A | - |
| MEK | A | D | A | A | A |
| Acetone | B | D | A | A | A |
| Chloroform | A | B | A | A | A |
| Ethylene Glycol | A | A | A | A | A |
| Mineral Oil | A | A | A | A | A |
| Gasoline | A | A | A | A | A |
| Diesel Oil | A | A | A | A | - |
| Lubricating Oil | A | A | A | A | A |
| Inorganics | |||||
| 3% Hydrogen Peroxide | A | B | A | - | B |
| Hydrogen Sulfide(Gas) | A | A | A | - | A |
| Aqueous | |||||
| Sodium Hypochlorite (Bleach) | A | A | A | A | C |
| Chlorine Aq. | A | A | A | D | A |
| Water | A | A | A | A | A |
| Note: To the best of our knowledge, the information contained in this guide is accurate, is based upon accepted technical practices and is believed to be reliable. Final determination of suitability of any process or material is the sole responsibility of the user. Extreme Bolt & Fastener, LLC does not assume any liability for the accuracy or completeness of this information. | |||||
| Comparison of Engineered Polymers | Victrex® PEEK | Kynar® PVDF | Teflon® PTFE / PFA | Torlon® PAI 4203 | Vespel® Polyimide |
|---|---|---|---|---|---|
| FDA | YES | YES | YES | NO | NO |
| USDA | YES | YES | NO | NO | NO |
| NSF | NO | YES | NO | NO | NO |
| 3A DAIRY | YES | YES | NO | NO | NO |
| USP CLASS VI | Medical Grades Available | YES | Medical Grades Available | NO | NO |
Engineered Polymers - Frequently Asked Questions
Answers from our engineers, drawn from the Engineered Polymers technical questions we're asked most.
Polymers at Cryogenic Temperatures
<u Polymers at Cryogenic Temperatures</u
Most often people want to know how hot a material can be used up to in an application, however for cryogenic applications, in media like liquified gasses (nitrogen, oxygen, carbon dioxide, LNG, etc.), we need to understand how materials perform at very cold temperatures. Polymer fasteners offer an excellent solution in cryogenic environments (including temperatures below -150°C) while minimizing thermal conductivity. As cryogenic applications grow, this area of engineering is finding its way into many industries such as:
• Supercomputers
• Pharmaceutical/biosciences applications
• Superconductors
• Magnetics
Benefits of Using Polymers in Cold Environments
• Low thermal conductivity
• Electrical insulating properties
• Sealing performance
• Ability to function as friction and wear surfaces without external lubrication
• Mechanically stable
That said, polymers do have their trade-offs at cryogenic temperatures. Generally, they become stronger, stiffer and harder – therefore less tough and hence more brittle. But even though their stiffness increases and impact strength is lowered at low temperatures, generally polymers will return to “normal” when heated up again.
Fluoropolymer for Low Temperatures
One class of polymers that excel at cryogenic temperatures are fluoropolymers. Examples of fluoropolymers are PVDF, PTFE and PFA. Like many materials they lose their flexibility at low temperature, but what is unique is that they retain their lubricity, abrasion resistance, and strength. Research has shown that PTFE that it is among the top fluoropolymers for cryogenics. PTFE can be used down to -328 °F (-200 °C) while showing little or no brittleness. It also remains highly flexible to nearly -100 °F below. While there are other fluoropolymers that can perform in extreme cold environments, they are not able to retain their material capabilities like PTFE.
Filled vs Unfilled Polymers
It’s important to point out that fiber reinforcements such as glass or carbon will make the polymers more brittle at cryogenic temperatures. However, if a polymer is being used for an application that involves large changes in temperature, it is a best practice to select a filled grade which will stabilize expansion. This chart shows that PEEK expands approximately 1% compared to only 0.3%. for 30% glass fiber reinforced PEEK.
Ductile / Brittle Transition Temperature Values
Which polymer do we offer that would have the smallest compressibility and minimal thermal expansion? We have a very precise laser application. So if the screw changes its dimensions with increasing / decreasing temperatures or loads their device may not be as accurate as it should be. Can you suggest a material that can work?
PEEK glass-fiber reinforced would be the best in terms of the Coefficient of expansion and compressibility.
I’m looking for threaded rods and nuts that would need to be able to withstand a potential exposure to ferric chloride and constant exposure to 3% hydrochloric acid which could reach 31% in a rare instance, would this PEEK withstand these chemicals?
PEEK fasteners work well with harsh chemicals. Regarding the HCl, PEEK threaded rod can handle the HCl is at ambient temperatures and a variety of PEEK can handle the concentrated 31% hydrochloric acid.
I need a bolt that can handle high temperatures and be an electric insulator? What can I use?
That depends on what you mean by high temperature and what other issues you have like the strength requirements. If you are talking about temperatures under 500F, then you may consider some engineered polymers. They are non-conductive both electrically and thermally. PEEK is the most economic choice up to about 500F. If you are talking about higher temperatures, then you would have to go with a ceramic like alumina which is an excellent insulatorand resistant to heat well over 2000F
I’m looking for a socket head cap screw that is 5/8″-11 x 5.5 inches in length. Need the material to be non-conductive and was thinking Ceramic Zirconia? Would that work?
Ceramics like Zirconia screws are in fact an excellent insulator from electrical current. However zirconia ceramic fasteners are very limited to smaller sizes between 2 – 1/4″ (M2-M6). Beyond this size they become very difficult to manufacture and are subject cracking. If electrical insulation is what you need, I would suggest a high performance polymer like PEEK socket head cap screws. PEEK is very economical compared to ceramics, an excellent electric insulator and can be made to just about any size. In addition, PEEK is tough, it will not be as fragile as a ceramic while offering the benefits of corrosion resistance and strength.
I’m building some lab equipment what will be housing hydrochloric acid. I need a non-metal fastener that is corrosion resistant . Can you make a recommendation?
In terms of a material that is not metallic and can handle hydrochloric acid, I would suggest either PTFE or PVDF. PTFE is virtually inert to most acids, as well as bases. If you laboratory is working on anything organic, it is bio-inert and will not leach into or contaminate sensitive scientific material. PVDF is also a good choice, as it offers similar resistance as PVDF to harsh chemicals, but with increased mechanical strength.
More on Engineered Polymers
What our customers say
More customer feedback“I purchased from you specifically because of Jon’s expertise and professionalism.”
“Very impressed; good prices and delivered earlier than lead time given, which was a real bonus.”
“Extreme Bolt is definitely on my go-to list.”