  • Monel 400 Bolts for Caustic Solutions?

    Q: I’m using a caustic soda solution to remove sulfur in a petroleum refinery. The steel bolts are NOT cutting it. Any suggestions? I don’t have a huge budget, so I’m hoping I don’t need Hastelloy or Tantalum fasteners?A: Nope…You don’t need anything that highly priced. For this situation Monel…

    Continue reading
  • Corrosion Resistant Fasteners for H2SO4 & Nitric Acid

    Q: I’m producing nitrobenzene to be used in dye manufacturing. The nitrobenzene is prepared by the nitration of benzene with a mixture of concentrated sulfuric acid, water, and nitric acid. I’ve tried Hastelloy C276 but its not working so well. A: Hastelloy C276 works very well in sulfuric acid which…

    Continue reading
  • Titanium or AL6XN Fasteners for Salt Water & Acids

    Q: We’re setting up a salt brine application for a chemical project. There may be some minimal exposure to some acids. Can I uses titanium bolts? A: Titanium Gr2 and Titanium Gr5 (6Al-4V) fasteners are excellent for almost all salt related environments, but here since you may have exposure to…

    Continue reading
  • Molybdenum bolts for high temperature furnace

    Q: I’m hoping you can help me with a high temperature issue. I’m running an ammonia plant where gases, along with hot air are heated to temps of 1800-2000F. The secondary reformer unit is made of carbon steel with refractory lining. I need bolting that can survive these temps so…

    Continue reading
  • A286 Bolts to Combat Stress Relaxing & Creep

    Q: Hi, I need a 1.25” X 15” bolt that can operate in continuous temperatures of 1000F. Currently we are using a heat treated carbon based 4140 fabricated machined bolt. At these temps the bolts are “Stress Relaxing” and we are losing our clamping pressure. In addition, when we change…

    Continue reading
  • Bolts for Hydrofluoric and nitric acid: Hastelloy & Monel

    Q: I’m running a chemical cleaning process on stainless steel to remove the oxides and to enrich the chromium depleted areas again surface. It’s an acid pickling process, where mixtures of hydrofluoric acid (HF) and nitric acid (HNO 3) are used. I’ve tried Hastelloy C276 bolting on my tanks because…

    Continue reading
  • Difference between Waspaloy and Inconel 718 fasteners

    I have a high temperature and strength application when would I choose Waspaloy bolts verses Inconel 718 bolts? Great question. Waspaloy and Inconel 718 bolts are both excellent in high temperature strength situations. In terms of strength, Inconel 718 has a edge over Waspaloy offering 210 ksi (ultimate tensile strength)…

    Continue reading
  • Hastelloy: Fasteners for phosphoric and sulfuric acid process

    Q: I’m using a pretty corrosive wet process to produce phosphoric acid. It involves taking phosphate rock and the addition of concentrated (93%) sulfuric acid in a series of well-stirred reactor. Any ideas on bolting that won’t corrode my bolts and fasteners? A: Since your process is exposed to both…

    Continue reading
  • Bolts for Steel Pickling in HCl: Hastelloy and Tantalum

    Q: I’m using HCl in a pickling process and have used Hastelloy C276 bolts to protect my equipment but am still having corrosion issues. Any ideas?A: In pickling processes ferric chloride is created which is a strong oxidizer and most pickling process are at elevated temperatures – Hastelloy C276 doesn’t…

    Continue reading
  • Hastelloy C276 Fasteners for Flue Gas Desulfurization Scrubbers

    Q: I’m operating a FGD (Flue Gas Desulphurization) plant and am experiencing some mild corrosion on my scrubber bolting. I’m currently using Incoloy 825 bolts. It’s mild corrosion but non-the-less I’d like to have it cleared up before I get additional issues. Any suggestions? A: Since scrubber liquids and gases…

    Continue reading
  • PEEK Screws for Steam & Radiation Sterilization Processes

    Q: I have a question regarding a type of fastener that can handle sterilization. What I need is a polymer if possible that can handle both steam and radiation sterilization processes, but doesn’t leach into my process. Contamination is an issue. A: You can definitely use a polymer for this…

    Continue reading
  • Over-sizing nuts to compensate for coated bolts

    Q: We have a corrosive application and we are debating on using coated carbon steel bolts and nuts or a solid corrosion resistant alloy. Obviously the coatings cost a lot less but we are unsure about how the coatings affect mechanical strength. A: Coated bolts and nuts are typically undersized…

    Continue reading
  • Hastelloy vs Tantalum Bolts for Sulfuric Acid Corrosion in Lithium Extraction

    Q: I’m running a lithium extraction process where a mineral called spodumene is roasted in a mixture of sulphuric acid (95-97%) at at about 150°C to form lithium sulfate. I’ve to use Hastelloy C276 for some process equipment but I’m still experiencing corrosion. Please help. A: Hastelloy C276 bolts typically…

    Continue reading
  • Galvanic corrosion between Inconel fasteners and Monel in seawater

    Q: I am considering using Inconel 718 fasteners with a Monel K-500 flange in seawater. I’m concered as Inconel is the more anodic of the two and is also has a smaller surface area. Would this cause galvanic corrosion? A: This is a great question. In this case if you…

    Continue reading
  • Hastelloy fasteners for HCL & H2SO4 in Municipal Waste Incinerator

    Q: I’m running a municipal solid waste incinerator and am having trouble corrosion from a combination of hydrochloric acid and sulfuric acid that is derived from chloride and sulfur containing compounds in the waste fuel stream. I was using Duplex steel bolts for the chloride corrosion but they aren’t holding…

    Continue reading