Galvanic compatibility of dissimilar metals

Galvanic Corrosion Chart

Galvanic Corrosion Risk
Metal in Contact
MagnesiumZincAluminum
Alloys
Carbon SteelCast IronLeadTinAustenitic Cast
Iron
BrassesGunmetal/Tin
Bronzes
Copper Nickel
Alloys
Nickel Alum
Bronze
Alloy
400/K500
Low Alloy
Stainless Steel
Nickel-Chrome
Moly Alloys
TitaniumHigh Alloy
Stainless Steel
Graphite
Fastener Material Being ConsideredMagnesiumAdditional corrosion unlikelyAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
ZincAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Aluminum AlloysAdditional corrosion may occurAdditional corrosion unlikelyAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Carbon SteelAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Cast IronAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
LeadAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
TinAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Austenitic Cast IronAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
BrassesAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Gunmetal / Tin BronzesAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAddition corrosion possibleAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Copper Nickel AlloysAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAddition corrosion possibleAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Nickel Alum BronzeAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAdditional corrosion may occur
Alloy 400 / K500Additional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAddition corrosion possibleAdditional corrosion may occur
Low Alloy Stainless SteelAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occurAdditional corrosion may occur
Nickel-Chrome Moly AlloysAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possibleAddition corrosion possibleAdditional corrosion may occur
TitaniumAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAddition corrosion possible
High Alloy Stainless SteelAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion may occur
GraphiteAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikelyAdditional corrosion unlikely
National Physical Laboratory

Chart Key

  • Additional corrosion unlikely
  • Additional corrosion may occur
  • Addition corrosion possible