A286 Bolts for High Temperature use with 409 Stainless
Q: I am working on two different exhaust systems based on 409 SS. I am looking for a 3/8-16 1” long bolt which can be fastened to threads in 409 SS. Currently, I am using Grade 8 bolts made from 300 M with Nickel Based Anti-Seize. The temperature can go…
Continue readingHastelloy for Formic Acid
Q: We are a producer of a preservative agent for livestock feed. Our process requires the use of formic acid. Any suggestions on an anti-corrosive bolt that can handle this acid?A: For formic acid I would typically suggest Hastelloy C276 or Hastelloy C22 but it always depends on concentration and…
Continue readingInconel Bolt for High Temperature Thermal Expansion
Q: I am looking for a bolt that will withstand working temperatures of around 800 degrees. We are having issues using grade 9 bolts that after multiple oven cycles we are having to cut the bolts off due to them being locked up. We need a bolt that will withstand…
Continue readingMonel Bolt for Anodizing
Q:We have an anodizing process that sends low voltage current through aluminum bars. We have been using 316 stainless bolts, but over time the electricity heats the bolts up red hot, then we lose clamping force. The tanks contain a solution of 15% sulfuric acid, so there is some corrosion…
Continue readingDIN 912 / ASTM A1082 / Super Duplex
Q: My customer is asking me to find them a Super Duplex bolt that meets DIN 912 and ASTM A1082. What does this mean and can you help out with this request.A: Yes, we can definitely help you with this request. Super Duplex is the type of material. The DIN…
Continue readingInconel Bolts & Alloy 330 Bolts for Cyclic High Temperature Conditions
Q: I need a material that can stay oxidation resistant at 2000F in a cyclic temperature environment. Any suggestions? A: One of the best choices is Inconel 601, UNS N06601,which is highly resistant to oxidation up to 2200°F and can handle even severe thermal cycling. These Inconel bolts will offer…
Continue readingA286 Protection From High Temperatures or Corrosive Conditions?
Q: I have an high temperature exhaust application that requires about 130ksi of tensile strength and is running pretty hot at 1000F. There are also some low concentration acidic contaminants that condense on the bolts during shutdowns, that have caused corrosion in the past on standard 316 bolting. Would A286…
Continue readingAlloy 20 vs Duplex Zeron 100 Bolts
Q: I was thinking of ordering some Duplex Zeron 100 bolts for some mild sulfuric acid. How does that compare to Alloy 20? My alloy 20 bolts are suffering some mild corrosion. A: Zeron bolts do offer a higher level of general resistance to corrosive environments compared to grades 2205…
Continue readingTitanium Grade 23 or TI 6AL-4V for Biocompatibility
Q: I’m working on a medical prototype that requires a strong bolt that is biocompatible. I know I want titanium but not sure which grade is adequate for medical use. A: Typically medical grade titanium screws are produced from grade 23 or TI 6AL-4V ELI or grade 5 6AL4V. A…
Continue readingAlloy 20 Bolts for Oxalic Acid
Q: Please recommend a material for use in 80 deg C oxalic acid solution. The titanium I’m using suffers, and dissolves. My hope is that C276 may work. We do not need high mechanical strength. I’m looking to order M4 and M6 socket head cap screws. A: Probably the best…
Continue readingDuplex Bolts versus 304 /316 Stainless Steel
Q: How does a Duplex screw compare to a stainless steel 300 series fastener? Would they be better in a saltwater environment? A: A Duplex stainless steel screw offers many advantages over 300 series stainless steel. Duplex is offered primarily in two grades Duplex 2205 and Super Duplex 2507 (with…
Continue readingA286 Bolts per ASTM A453 660
Q: I have a high temperature exhaust stream that is part of an air-to-air energy recovery system that experiences temperatures around 1300F consistently and can go up to 1500 intermittently. I need to ensure that the bolts have a tensile strength of 130ksi. Can you help me out with this?A:…
Continue readingHastelloy C276 Bolts versus Nickel 200 Bolts
Q: Because Nickel 200 bolts have much higher nickel content than Hastelloy C276 does that mean they are more corrosion resistant than a Hastelloy bolt?A: No. Though nickel content plays a huge role in corrosion resistance, however there are other elements that contribute to the high level of corrosion protection…
Continue readingCoefficient of Thermal Expansion (CTE): TZM vs Tungsten
Q: I’m working with a high temperature, bi-metallic bolted flange design. The steady state temperature of the flange is 1400 degrees F. The bolt is TZM, which has a lesser CTE than the thru-hole material. I’m looking for a material with a CTE less than TZM to use as a…
Continue readingTitanium Grade 5 versus Aluminum
Q: What is the difference between using aluminum compared to a titanium bolt for a medical fastener? A: Medical grade titanium bolts – grade 5 – have an incredible strength to weight ratio. They are 60% denser than aluminum but more than twice as strong. This makes a titanium boltexcellent…
Continue reading