Technical Questions – FAQ’s
Last updated
463 posts · page 29 of 31
Yield strength difference between MP35N and A286 bolts
Q: I need high yield strength material what is the difference between MP35N and A286? Which is more economic? A: Overall MP35Nis perhaps the highest yield strength bolt material available to industry with a typical yield of 250 ksi compared to A286’s 111 ksi; though it is extremely expensive. A286…
Continue readingBolt for hot hydrogen sulfide, CO2, hydrocarbons & salt water
Q: I need a material that will be suitable for oil and gas use. Submersion in hydrogen sulfide, carbon dioxide, hydrocarbons, salt water at temperatures up to 325F. Crevice corrosion has been a factor. Also need 170ksi min tensile strength. Plus we’d like to torque a 3/8-24 fastener to 50…
Continue readingFastener for cyrogenic application
Q: I need to attach an LNG cryogenic pump and need to make sure I use a material that can withstand temperatures of –120 °F as well as don’t embrittle when fluctuating back to room temperature. Any suggestions? A: Monel K500 is a common choice for cyrogenic fasteners. It can…
Continue readingHastelloy C276 bolts in hot sulfuric acid
Q: I was planning on using Hastelloy C276 in hot sulfuric acid. It would be approximately 50% concentration around 100F +/- 10 degrees. Will this be okay? I’m just concerned because I read that it cannot handle strong oxidizing environments and I’ll be using it in an application where its…
Continue readingPolymer screw for high vacuum, usable to 150C
Q: I have an application where I need pan head, insulating, high vacuum compatible, screw. It will also need to be usable at a service temperature up to 150C. Do I need a ceramic? A: Though ceramics are excellent insulators, they are usually only used for high temperature applications, where…
Continue readingHastelloy C22 bolts for hydrochloric acid steel pickling
Q: We are running a steel pickling process are considering switching from a sulfuric acid process to hydrochloric acid. Our system currently uses Inconel 625 bolting. With this be sufficient? A: Inconel 625is a good material for acid corrosion but for large system of hydrochloric acid, especially with the corrosion…
Continue readingWhy ceramic bolts don’t have yield strength
Q: I was looking at your site and noticed that the ceramics don’t have a yield strength. What does that mean?A: Metals and plastic have yield strengths because they start to stretch before breaking… the point where they start stretching is the “yield point” and the stress at that point…
Continue readingPolymer screw resistant to chlorine and chlorine dioxide
Q: I’m looking for a chemically resistant polymer that can withstand chlorine and chlorine dioxide as well as a decent amount of weight and tension (around 27 lbs of weigh). Can you suggest a material? A: Of course it depends on the concentrations and temperatures you are operating at but…
Continue readingEmbrittlement of Tantalum bolts at high temperatures
Q: I chose Tantalum bolts for their corrosion resistance and high temperature capabilities and they are breaking. I’m running an application that fluctuates between 350 Celcius where there could be concentrated sulfuric acid contamination. I thought these would be excellent with high temperature acid exposure. Can you help me? I…
Continue readingDuplex 2507 bolts for salt air corrosion resistance
Q: I’m working on a structural project that not submerged in salt water but exposed to moist salt air. I’m not only concerned about the supports having fasteners that won’t corrode but also having a fastener that is high strength. Any suggestions. A: Though I don’t know the specific strength…
Continue readingZirconium fasteners exposed to downstream oxidizers
Q: I’m using zirconium fasteners in a sulfuric acid process but they are showing corrosion. I’m not sure why as I’m well below boiling and only using 40% concentration. There may be some downstream contaminants, but not much. Any ideas? A: It is most likely the contaminants that are causing…
Continue readingDuplex bolts in sea water contaminated steam turbine
Q: I’m running a steam surface condenser which is installed on a steam turbine in a thermal power station. I’m using sea water that could be contaminated with chemical pollutants cooling water side of the condenser. Any ideas on a good fastener for the tubes and water boxes? A: Duplex…
Continue readingTantalum vs Monel fasteners in hydrogen fluoride
Q: I’m using hydrogen fluoride used in a manufacturing process to make refrigerants. I know it’s very corrosive and have tried both hastelloy and inconel fasteners, which I thought were super corrosion resistant. What am I doing wrong because the acid is still eating them? Should I try Tantalum?A: Definitely…
Continue readingDuplex 2507: Bolts for geothermal drilling exposed to sulfur and salt
Q: I’m working on a on a geothermal energy drilling project. Carbon steel we’re currently using to bolt drilling components is failing from corrosion. We have corrosive an environment with high levels of sulfur and salt, as well as temperatures to 260C. Any suggestions? A: Super Duplex 2507 is often…
Continue readingBest bolts for Inconel 625 flanges
q: What bolting material should be used with Inconel 625 flanges? We used ASTM A193 Gr B7 however noticing some corrosion issues.A: This is a very common problem but to answer it accurately, it depends on the environment that your flangessee and also to a certain extent what media is…
Continue reading