  • Bolts for municipal waste incinerator: Hastelloy protects from HCl corrosion

    Q: I’m running a municipal solid waste incinerator and am having trouble with corrosion from a combination of hydrochloric acid and sulfuric acid that is derived from chloride and sulfur containing compounds in the waste fuel stream. I was using Duplex steel bolts for the chloride corrosion but they aren’t…

    Continue reading
  • Titanium bolts: Light weight fasteners that are stronger than aluminum

    Q: I have a lightweight application that requires high strength. I’ve tried aluminum screws because I thought they were ultra lightweight but after breaking I increased my bolt size and now I have more weight and still breakage. No sure what to do. A: Yes aluminum is a lightweight material…

    Continue reading
  • PEEK screws for high temperature to 400F & corrosion resistance

    Q: I’m designing laboratory equipment that will be utilized at 325-400F and I need screws that have immunity to organics and low concentrations of acids, as well be FDA approved. Would that be a ceramic? A: You probably don’t want a ceramic screw. Though they are corrosion resistant and offer…

    Continue reading
  • Inconel & Alloy 330 bolts for high temperature strength

    Q: My customer is having an issue with his stainless steel fastener bending. They are being used in a high-heat application running at approximately 1600F. Is this normal? Any ideas? A: This is definitely expected at these temperatures. If temperatureand strength are you main focus, I would suggest either Inconel600…

    Continue reading
  • Hastelloy bolts for hydro-treating with sour gas – H2S

    Q: I’m running a hydro-treating process that is running at 350-390°C where we’re producing H2S and NH3. Any ideas on a bolt that can handle the temperature and chemicals? A: In this type of process you having to deal with high temperatures and the formation of sulfuric acid (H2SO4) from…

    Continue reading
  • Duplex 2507 bolts for high strength application in salt air

    Q: I have a high strength application that requires resistance to damp salt air and occasional sea splash, I’m using Monel 400 but it’s not holding up the the 75ksi of yield I need. Lots of broken bolts? Is is corrosion or strength? Thoughts? A: Your issue isn’t the corrosion.…

    Continue reading
  • AL6XN vs Monel bolts for salt water and marine use

    Q: Is AL6XN a steel or nickel alloy? Trying to figure out if it would perform as well as Monel in seawater. A: To answer your first question, AL6XN bolts are actually both a nickel and a steel alloy. AL6XN is often described as a high nickel content stainless alloy.…

    Continue reading
  • Incoloy 825 vs Hastelloy C276 for Sour Gas

    Q: I need bolts for a well pump exposed to sour gas? I’ve currently use Incoloy 825 bolts which works reasonably well, but I’m wondering if there is a better choice that is more economical and could offer equal or better corrosion resistance – any ideas? A: A great nickel…

    Continue reading
  • Bolt resistant to sodium hypochlorite with 80ksi yield strength

    Q: I’m looking for guidance on fasteners with good resistance exposure to sodium hypochlorite. The material would need to be bleach-resistance, but also have a tensile yield strength of over 80ksi. A: For sodium hypochlorite applications that are often used for municipal water treatment titanium, fasteners are an excellent choice.…

    Continue reading
  • High temperature fastener for furnace up to 3000F

    Q: I am looking for a suitable fastener for use in a high heat furnace that is running at 2000F but the actual hearth wear flames go up to 3000F. The furnace is not under vacuum and has a normal atmosphere. We are finding that the 304 bolts are failing…

    Continue reading
  • High temperature bolt for sulfur & chloride gas corrosion resistance

    Q: I have a high temperature application which is exposed to sulfur and chloride gasses. We’re operating at between 1200° and 1400°F. Any suggestions on a bolt material to consider? A: To deal with both sulfuric/chloride atmospheres as well as high temperatures, you may want to consider Incoloy 800HT bolts…

    Continue reading
  • Non-metal fastener for hydrochloric acid

    Q: I’m building some lab equipment what will be housing hydrochloric acid. I need a non-metal fastener that is corrosion resistant . Can you make a recommendation? A: In terms of a material that is not metallic and can handle hydrochloric acid, I would suggest either PTFE or PVDF. PTFE…

    Continue reading
  • Corrosion resistance of Inconel 625 bolts vs Hastelloy C276

    Q: Inconel 625 and Hastelloy C276 bolts seem to have similar Nickel content. Does this mean these fasteners will perform the same in a corrosive environment? A: Inconel 625 and Hastelloy C276 bolts do offer similar corrosion resistance but Hastelloy C276 has a slight edge in many acidic environements, especially…

    Continue reading
  • Alloy 20 fasteners for sulfuric acid corrosion

    Q: I’m working with boiling sulfuric acid and tried Alloy 20 for some of my bolting but am having corrosion. I’m confused as I thought that is what they are best for. Any suggestions. A: You are right Alloy 20 does typically perform very well in sulfuric acid and even…

    Continue reading
  • Incoloy 925 bolts for sour gas & chloride application

    Q: I have down hole application containing sour gas and high chloride levels. The temperature the bolts are exposed to is around 150F and I’m having trouble with cracking. I tried Super Duplex 2507 but am still having issues. Any ideas? A: Super Duplex 2507 does provide good resistance to…

    Continue reading