Technical Questions – FAQ’s
Last updated
463 posts · page 16 of 31
Nitronic 60 vs A286 for High Temperatures
Q:How does Nitronic 60 compare to an A286 bolt for high temperature strength? A: That depends on the strength required and the temperature of your application. A Nitronic 60 bolt is known for its high temperature properties up to 1800F. At these extreme temperatures it can offer good resistance to…
Continue readingSuper Duplex for Structural Project in Salt Air
Q: I’m looking for a bolt that can handle salt air and be structurally sound with a tensile strength of about 115-120 ksi max – do I require a titanium grade 5 bolt because I know they are costly?A: Probably not at that tensile strength. A Super Duplex bolt may…
Continue readingTitanium Bolts for High Strength Chloride Application
Q: I have a chlor alkali application that requires high strength of about 110ksi of tensile strength. Heat is not a factor but I’m concerned about the strength. Can you make any recommendations? A: For chlor alkali services one of the best materials is titanium. While a standard titanium grade…
Continue readingA Duplex Bolt vs AL6XN in Saltwater
Q: How does a Duplex bolt compare to AL6XN in a hot saltwater situation?A: Duplex bolts are ideal for chlorides and mild saltwater application such as brackish water, salt air and moderate temperature unpolluted seawater. An AL6XN boltwill provide more corrosion protection than a Duplex bolt in marine and salt…
Continue readingMonel 500 Bolts for Hydrofluosilicic Acid
Q: What is the best alloy to bolt to use in a flange on the outside Hydrofluosilicic acid storage tank? A: Probably the best materials for Hydrofluosilicic acid bolting would be a Monel K500 bolt. This material will give you the strength and good corrosion resistance to the this very…
Continue readingAlloy 20 Bolts and Inconel Bolts for Downhole Oil Application
Q: Hi there! I have a set screw in a downhole Oil and Gas application that is experiencing cam out/stripping and seeking a recommendation for a drop in replacement. With 17-4 and stainless steel, galling is a real issue for us. Also with the application being down-hole, if the screw…
Continue readingAn Inconel 600 Bolt vs an Inconel 625 Bolt
Q: Does Inconel 600 provide the same level of corrosion resistance as an Inconel 625 bolt?A: Not typically. For corrosion resistance, an Inconel 625 boltis one of the more corrosion resistant versions of the Inconel alloys and it can withstand many strong hot acids. While not as corrosion resistant as…
Continue readingHastelloy C276 Bolts for Hot Acids
Q: I’m running a laboratory process that will be exposing bolts to a variety of acids. I’d like a metal bolt that can withstand low concentration hot acids. I was thinking a Hastelloy C276 bolt may be a good option. Are there any acids I should beware of that can…
Continue readingCarburization Resistant Bolts
Q: It says that Alloy 330 is carburization resistant. What does that mean exactly? A: Carburization is when heat hardens a metal. Carburizing is sometimes used in alloy aging processes when your goal is to harden the alloy. On the other hand unwanted carburization can occur at extreme temperatures which…
Continue readingOxidation Resistant A286 and Alloy 330 Bolt
Q: I was reading that high temperatures will accelerate the rusting of metal bolts. Is there a material that can prevent this. I’m using the screws at 1300F intermittently.A: What you are looking for is an oxidation resistant bolt. When a metal oxidizes it is attacked by oxygen which accelerates…
Continue readingHastelloy and Inconel Bolts for High Temperature & Low Acidic Environments
Q:We are currently using mild steel with a black oxide coating and the bolts are breaking down because they are stretching under tension because of the heat, and corrode in various places from our acids.The acids we use here are Hydrochloric (HCl) and Sulfuric (H2SO4), both are heavily diluted with…
Continue readingTitanium vs Monel 400 for Polluted Stagnant Seawater
Q: I’ve been using Monel 400 bolts for a coastal operation that is built in polluted, stagnant saltwater. I’m been having some slight corrosion – nothing drastic, but wanted to check if there was another material that would last longer. A: For this situation I would suggest titanium bolts. Titanium…
Continue readingHastelloy C276 vs. Hastelloy C22 Fasteners
Q: What’s the difference between Hastelloy C276 and Hastelloy C22?A: Hastelloy C276 fastenersoffer very good resistance to strong reducing corrosive acids, as well excellent stress corrosion cracking resistance and resistance to localized attack. They are renowned for their corrosion resistance to various concentrated, hot acids and reducing environments, and are…
Continue readingWill A286 Fasteners Gall with Titanium or Stainless
Q: I want to use A286 fasteners with our product (a force sensor). Will A286 gall with 6Al4V titanium or 15-5 stainless steel or 304 SS helicoils without lubrication. The customer will not allow lubricants. Thank you A: The biggest factor to galling is using similar material on each other.…
Continue readingBleach Plant: Titanium vs Hastelloy C276
Q: We need bolts for a shutdown in our Bleach Plant where Chlorine Dioxide is the attacking agent. Is titanium sufficient or should we be using C276 bolts? A: Titanium bolts are typically more than sufficient. Titanium fasteners are renowned for their resistance to chlorides and chlorines – they are…
Continue reading