MP35N Hex Head Bolts
Last updated
One of the highest strength alloys available to industry
Need help choosing a material?
- Extreme high strength properties with a min 260ksi ultimate tensile.
- Good in moderately elevated temperatures of 800°F.
- Moderate corrosion resistance.
- MP35N chemisty, specs, and heat treatments
- Datasheet for MP35N
- MP35N hex head cap features and benefits
MP35N hex head bolts are known for their extraordinary strength and are the strongest bolts we offer at Extreme Bolt. MP35N bolts owe their extraordinary strength to a unique alloy combination of nickel, cobalt, chrome and molybdenum. These fasteners have a minimum 260ksi ultimate tensile strength, which typically reaches ~285ksi.
Beyond the strength of MP35N hex head bolts, they are also exhibit good corrosion resistance and can resist most mineral acids, hydrogen sulfide, seawater and salt spray environments.
MP35N bolts are also resistant to high temperature oxidation and could operate in environments up to 800°F and still maintain much of its strength.
Applications where MP35N hex head bolts are often found are: aerospace, defense, marine, chemical processing, oil and gas and medical.
Bolt Types Available: Hex Bolts, Shoulder Bolts
MP35N Hex Head Bolt Features and Benefits
It is important to differentiate between a MP35N hex head bolt and hex head cap screw. Often people assume they are the same, but they are actually very different fasteners in terms of how they are manufactured, as well as from an application perspective. Regardless of your choice, MP35N hex heads offer strong, stable joints because of their large head service.
The Hex Comparison
|
Hex Head Bolts |
Hex Head Cap Screw |
|
|
MP35N Chemistry, Spec and Heat Treatments
Heat Treating & Aging: MP35N is usually supplied in heat treated and cold drawn condition AMS 5844. In this state the MP35N can be worked into the desired fastener form and aged to the AMS 5845 specification. Once aged, the MP35N material could achieve it full strength potential.
MP35N Specifications: AMS 5844, AMS 5845, AMS7468, ASTM F562, NACE MR0175
| MP35N | Ni | Co | Cr | Mo |
|---|---|---|---|---|
| Typical % | 35 | 35 | 20 | 10 |
| Guarenteed Minimum Properties | Nominal Properties | |||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| UTS (ksi) | Yield Strength (0.2%) ksi | Elongation (% 4D) | RA (%) | HRC | UTS (ksi) | Yield Strength (0.2%) ksi | Elongation (% 4D) | RA (%) | HRC | |
| MP35N Cold Drawn Full Strength | 260 | 230 | 8 | 35 | 44 min | 285 | 275 | 9 | 45 | 50 |
| Media | Corrosion Resistance | Media | Corrosion Resistance |
|---|---|---|---|
| Nitric Acid | Good | Sulfuric Acid | Good |
| Phosphoric Acid | Good | Acetic Acid | Excellent |
| Sodium Hydroxide | Good | Salt Spray (NaCl) | Excellent |
| Sea Water | Excellent | Sour Oil/Gas | Excellent |
| Important Note: The following 4-level rating scale is intended for comparative purposes only for this materials only. Corrosion testing is recommended; factors which affect corrosion resistance include temperature, concentration, pH, impurities, aeration, velocity, crevices, deposits, metallurgical condition, stress, surface finish and dissimilar metal contact. | |||