C22 nickel alloy screws offer better overall corrosion resistance to its sister alloy Hastelloy C-276, more specifically, it provides better protection when used in certain saturated wet chlorine environments. In addition, its high chromium content provides C22 screws much better resistance to oxidizing media that C276. This provides it exceptional resistance to chloride-induced pitting although, in most cases because of its availability, C-276 screws are a more cost-effective option especially in sizes less than 1/2". Hastelloy C22 screws are best known for its resistance to pitting and crevice corrosion – which is unmatched in the high performance nickel alloy class. Use of C22 screws should be limited to temperatures below 1250°F due to the formation of detrimental phases which form above this temperature. Click for detailed chemistry and specifications information on Hastelloy C22 nickel alloy screws. C22 mechical properties and tensile data is also available.

Availability: Hastelloy C22 screws are generally available in 1/2" sizes and larger due to materials availability. Most C22 screws are made to order.

Corrosion Performance

Key Benefits

  • Alloy C-22 screws have outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking
  • Extremely high protection from wet chlorine environments
  • Excellent resistance to a wide variety of chemical process environments including strong oxidizers such as ferric acids, acetic anhydride, hot contaminated media (organic and inorganic), and seawater and brine solutions
  • Similar overall corrosion protection compared to C276
  • Very ductile, exhibits excellent weldability

Welding

Alloy C22 is considered the best alloy to use as universal weld filler metal to resist corrosion of weldments. These C22 screws will resist the formation of grain boundary precipitates in the weld heat zone, which make them ideal most chemical process applications in the welded condition.

Uses

  • Hastelloy C22 screws protect extensively against the most corrosive flue gas desulfurization systems and the most sophisticated pharmaceutical reaction vessels
  • Chemical process industries depend on C22 screws for use in equipment like flue gas scrubbers, chlorination systems, sulfur dioxide scrubbers, pulp and paper bleach plants, pickling systems, and nuclear fuel reprocessing

Flange Types Available: Blind Flanges, Lap Joint Flanges, Slip On Flanges, Socket Weld Flanges, Threaded Flanges, Weld Neck Flanges


Hastelloy C22 Screws Chemistry & Specifications

C22 alloy, UNS N06022, has better overall corrosion resistance in oxidizing corrosives than C-276 and Inconel 625 alloys due to the higher chromium content. Outstanding resistance to localized corrosion and excellent resistance to stress corrosion cracking. This alloy has limited availability and can be made into fastener in larger diameters only (1/2" and greater in size). 

Hastelloy C22 Specifications: SB 575/B 575, SB 574/B 574, SB 366/B 366 SB 462/B 462, SB 564/B 564 SB 462/B 462, 17744 No. 2.4602 NiCr21Mo14W, NACE MR0175 ISO 15156, Werkstoff 2.4602

Hastelloy C22 — table
Hastelloy C22NiMoCrFeWCoMnCuVSiC
Nominal %56 BAL13.022.03.03 Max2.5 Max0.5 Max0.5 Max0.35 Max0.08 Max0.01 Max

MECHANICAL PROPERTIES OF HASTELLOY

C22 Tensile Data


Hastelloy Corrosion Data

AQUEOUS CORROSION RESISTANCE OF NICKEL ALLOYS
MediaConcentration,
Percent
By Weight
Test
Temperature
°F (°C)
Average Corrosion Rate Per Year, mils*
625 alloyC-22® alloyC-276 alloyG-30® alloy
Acetic Acid99Boiling<1Nil<11
Ferric Chloride10Boiling732512--
Formic Acid88Boiling9<112
Hydrochloric
Acid
1Boiling13131
1.5Boiling3531432--
2194 (90)NilNil1--
2Boiling5576151--
2.5194 (90)72<112--
2.5Boiling60514185--
10Boiling6424002882364
Hydrochloric Acid
+ 42 g/l Fe2(SO4)3
1200 (93)238241803
5150 (66)225557
Hydrochloric Acid
+ 2% HF
5158 (70)123592697
Hydrofluoric
Acid
2158 (70)209910
5158 (70)16141011
P2O5
(Commercial
Grade)
39185 (85)129--
44240 (116)2321100--
52240 (116)121133--
P2O5 + 2000 ppm Cl38185 (85)2112--
P2O5 + 0.5% HF38185 (85)9745--
Nitric Acid10Boiling<1<17<1
65Boiling211348885
Nitric Acid + 6% HF5140 (60)7367207--
Nitric Acid + 25% H2SO4
+ 4% NaCl
5Boiling7131264--
Nitric Acid + 1% HCl5Boiling1<18--
Nitric Acid + 2.5% HCl5Boiling<1221--
Nitric Acid + 15.8% HCl8.8126 (52)>10,00043314
Sulfuric Acid10Boiling37121931
20150 (66)<1<1<1--
20174 (79)<113<1
20Boiling91333954
30150 (66)<1<11<1
30174 (79)<134<1
30Boiling227645560
40100 (38)<1<1<1<1
Sulfuric Acid40150 (66)1<11<1
40174 (79)359102
50100 (38)1<1Nil<1
50150 (66)2514<1
50174 (79)58161210
60100 (38)<1<1<1<1
70100 (38)<1NilNil<1
80100 (38)<1Nil<1--
Sulfuric Acid + 0.1% HCl5Boiling1512633--
Sulfuric Acid + 0.5% HCl5Boiling4346149--
Sulfuric Acid + 1% HCl10158 (70)121<111--
10194 (90)3269445--
10Boiling869225116--
Sulfuric Acid + 2% HF10Boiling55292253
Sulfuric Acid +
200 ppm Cl-
25158 (70)1101112--
25Boiling325215186101
Sulfuric Acid +1.2% HCl
+ 1% FeCl3 + 1% CuCl2
11Boiling18153421227
Sulfuric Acid +1.2% HCl
+ 1% FeCl3 + 1% CuCl2
(ASTM G28B)
23Boiling2721855--
Sulfuric Acid +42 g/l
Fe2(SO4)3 (ASTM G28B)
50Boiling23402507
*To convert mils per year (mpy) to mm per year, divide by 40

Hastelloy C22 Sulfuric Acid Corrosion Performance

Hastelloy C22 - resistance to sulfuric acid (iso-corrosion diagram)


Hastelloy C22 Hydrochloric Acid Corrosion Performance
Hastelloy C22 - resistance to hydrochloric acid (HCl)


Hastelloy C22 Nitric Acid Corrosion Performance

Hastelloy C22 - resistance to nitric acid (iso-corrosion diagram)


Hastelloy C22 Phosphoric Acid Corrosion Performance

Hastelloy C22 — resistance to phosphoric acid

Questions?

Our material experts are ready to help guide you through your specific application.